• Promoted and Thixotropy Unsaturated Polyester Resin
  • Promoted and Thixotropy Unsaturated Polyester Resin
  • Promoted and Thixotropy Unsaturated Polyester Resin
  • Promoted and Thixotropy Unsaturated Polyester Resin
  • Promoted and Thixotropy Unsaturated Polyester Resin
  • Promoted and Thixotropy Unsaturated Polyester Resin

Promoted and Thixotropy Unsaturated Polyester Resin

CAS No.: 100-42-5
Formula: (C8h4o3.C4h10o3.C4H2O3)X
EINECS: 1866
Molecular Principal Chain: Element Organic Polymer
Color: Light Yellow/Purple
220kg/Drum: 80 Drum in 20FCL
Samples:
US$ 1.1/kg 1 kg(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2013

Suppliers with verified business licenses

Jiangsu, China
to see all verified strength labels (12)
  • Overview
  • Product Description
  • Detailed Photos
  • Packaging & Shipping
Overview

Basic Info.

Model NO.
GP191
Shelf Time
3 Month
Transport Package
Drum
Specification
A Grade Quality
Origin
China
HS Code
39079100
Production Capacity
10000ton/Year

Product Description

 
Product Description

 191 is an orthophthalic based polyester general-purpose resin. It have several different variants:

    1, 191(LSE) is an environment friendly variant of 191. Compared with 191, the LSE variant has lower styrene emission which could protect the employees who need to apply it in the closed space.
    2, 191P is pre-promoted 191 resin. The color of 191P is pink, while the 191 is yellow.
    3, 191TP is thixotropic and pre-promoted 191 resin. It is pink troubled liquid.
 
Potential applications:
    1, Boat Construction
    2, Pultrusion and RTM
    3, Filament Winding Pipe
    4, SMC/BMC
    5, Painting
    6, Translucent Panel

Geltime Table:
Ambient Temperature 25ºC 30ºC 30ºC
Catalyst M50 2% V388 1% V388 1.2%
Viscosity (Pas) 500-550 400-450 400-450
Thixotropic Index 2.2-3.0 2.1-2.6 2.1-2.6
Gel Time (min) 21 36.6 31

Properties of Resin Casting Bodies (for reference):
Projects Measured value Test method
Barcol hardness 43 GB 3854-83
Thermal deformation temperature (ºC) 68 GB 1634-04
Flexural strength (Mpa) 112 GB 2570-95
Tensile strength (Mpa) 70 GB2568-95
Elongation (%) 3.5 GB2568-95
Impulse strength (kJ/m2) 10.2 GB2571-95
Note: (1), The method of casting bodies making sample must be implemented based on GB 8237-87
          (2), Curing conditions: MEKPO 2%; promoter 2% (cyclohexanone peroxide)
          (3), Curing time: 60ºC×2 hour + 80ºC×2hour


Properties of Fiberglass Reinforced Plastic (for reference):
Porjects Measured value Test method
Flexural strength (Mpa) 365 GB/T1449-83
Flexural Modulus (Mpa) 290 GB/T1447-83
Impulse strength (kJ/m2) 235 GB/T1451-83
Note: (1), The method of fiberglass reinforced plastic making sample must be implemented based on GB 8237-87
          (2), Curing conditions: MEKPO 2%; promoter 2% (cyclohexanone peroxide)
          (3), Curing time: 60ºC×2 hour + 80ºC×2hour


Transportation and Storage:
The transportation shall comply with the chapter V of the Regulations on Measures for the Administration of Road Transportation Safety of Dangerous Goods.

    1, Store below 25ºC
    2, Avoid direct sunlight, fire and heat.
Detailed Photos

 

Promoted and Thixotropy Unsaturated Polyester Resin
Promoted and Thixotropy Unsaturated Polyester Resin
Packaging & Shipping
Promoted and Thixotropy Unsaturated Polyester Resin
Promoted and Thixotropy Unsaturated Polyester Resin

Give us a chance, and we' ll return you with satisfaction. 